What Temperature Will My Parts See During the Parylene Coating Process?
Posted by Sean Horn on Fri, Nov 13, 2020
Parylene coating process involves 3 steps: sublimation, pyrolysis, and polymerization. At the first step, which takes place between 120°C – 175°C, the dimer parylene powder precursor is sublimized and pyrolysed forming the monomers (see Figure). Next, Pyrolysis takes place which is defined as the thermal decomposition of materials at elevated temperatures (above 500 °C) in […]